dc.identifier.citation |
Прочность и микроструктура паяных соединений сплава ЖС6У, полученных с использованием комплексных бор- и кремнийсодержащих припоев / А.Ф. Белявин, В.В. Куренкова, И.С. Малашенко, В.В. Грабин, В.В. Трохимченко, Л.В. Червякова // Современная электрометаллургия. — 2010. — № 2 (99). — С. 40-51. — Бібліогр.: 17 назв. — рос. |
uk_UA |
dc.identifier.issn |
0233-7681 |
|
dc.identifier.uri |
http://dspace.nbuv.gov.ua/handle/123456789/96135 |
|
dc.description.abstract |
Рассмотрена взаимосвязь микроструктуры металла паяного шва и физико-механических свойств соединений сплава ЖС6У, полученных с применением комплексных бор- и кремнийсодержащих припоев, в которых в качестве наполнителя использовали 60 мас. % порошка сплава Rene-142. Показано, что введение в базовый припой Ni—Co—Cr—Al—2,5 % B + Rene-142 2,4… 3,0 мас. % кремния вызывает изменение морфологии и количества выделяющихся карбоборидных фаз. Приведены результаты высокотемпературной пайки литых пластин из сплава ЖС6У, рассмотрена структура паяных соединений, их прочностные и пластические характеристики при температуре 20 °С. Добротность паяных соединений составляет 0,85… 1,00 прочности базового сплава. Особое внимание уделено влиянию зазоров на результаты механических испытаний паяных соединений сплава ЖС6У при растяжении. |
uk_UA |
dc.description.abstract |
Considered is the interrelation between the microstructure of metal of brazed joint and physical-mechanical properties of joints of alloy ZhS6U, produced using complex boron- and silicon-containing brazing alloys, in which 60 mass % of powder of alloy Rene-142 was used as a filler. It is shown that the adding of 2.4… 3.0 mass % of silicon into basic brazing alloy Ni—Co—Cr—Al—2.5 % B + Rene 142 causes the change in morphology and amount of evolving carbide-boride phases. The results of high-temperature brazing of cast plates of ZhS6U alloy are given, the structure of brazed joints, their strength and ductile characteristics at temperature 20 °С are considered. Quality of brazed joints is 0.85… 1.00 of strength of the basic alloy. A special attention is paid to the effect of gaps on the results of mechanical tests of brazed joints of alloy ZhS6U at tension. |
uk_UA |
dc.language.iso |
ru |
uk_UA |
dc.publisher |
Інститут електрозварювання ім. Є.О. Патона НАН України |
uk_UA |
dc.relation.ispartof |
Современная электрометаллургия |
|
dc.subject |
Общие вопросы металлургии |
uk_UA |
dc.title |
Прочность и микроструктура паяных соединений сплава ЖС6У, полученных с использованием комплексных бор- и кремнийсодержащих припоев |
uk_UA |
dc.title.alternative |
Strength and microstructure of ZhS6U alloy brazed joints produced using complex boron- and silicon-containing brazing alloys |
uk_UA |
dc.type |
Article |
uk_UA |
dc.status |
published earlier |
uk_UA |
dc.identifier.udc |
621.791.3.05.011:539.2:620.17 |
|