Показати простий запис статті
dc.contributor.author |
Sobol`, O.V. |
|
dc.date.accessioned |
2018-06-16T17:46:23Z |
|
dc.date.available |
2018-06-16T17:46:23Z |
|
dc.date.issued |
2007 |
|
dc.identifier.citation |
Thermal factor effect on phase formation, structure, substructure features, and stress state in ion-plasma nano-crystalline condensates of quasi-binary WC-TiC carbide / O.V. Sobol` // Functional Materials. — 2007. — Т. 14, № 4. — С. 436-445. — Бібліогр.: 17 назв. — англ. |
uk_UA |
dc.identifier.issn |
1027-5495 |
|
dc.identifier.uri |
http://dspace.nbuv.gov.ua/handle/123456789/136915 |
|
dc.description.abstract |
Using high-angle X-ray diffraction and X-ray fluorescence spectral analysis, the effects of the sputtered material composition and deposition temperature on the phase and elemental composition, structure, substructure features, and stress state in the ion-plasma quasi-binary WC—TiC coatings. The increase in relative titanium atomic content has been established to result in increasing thermal stability of the single-phase state of the ((W,Ti)C solid solution) condensate up to the temperatures exceeding 950°C at the atomic ratio Ti/W≥0.35. At atomic ratios Ti/W≤0.25 and deposition temperatures exceeding 800°C, a multi-phase condensate is formed containing the lower carbide W₂C, the essentially pure α—W phase with the BCC lattice, along with WC and TiC phases formed through (W,Ti)C solid solution decomposition. In the range of the single-phase solid solution formation, the crystallite sizes rise and the micro-strain extent drops as the condensation temperature rises. The transition into the temperature range of the multi-phase coating is followed by the micro-strain increase and the average crystallite size diminution. The carbon content in the (W,Ti)C solid solution has been estimated and the critical deposition temperature established to be 700°C; at higher temperatures, intensive vacancy formation occurs in carbon sublattice of the carbide. Physical reasons for the effects observed and the regularities revealed have been discussed. |
uk_UA |
dc.language.iso |
en |
uk_UA |
dc.publisher |
НТК «Інститут монокристалів» НАН України |
uk_UA |
dc.relation.ispartof |
Functional Materials |
|
dc.subject |
Characterization and properties |
uk_UA |
dc.title |
Thermal factor effect on phase formation, structure, substructure features, and stress state in ion-plasma nano-crystalline condensates of quasi-binary WC-TiC carbide |
uk_UA |
dc.title.alternative |
Вплив термічного фактора на процес фазоутворення, структуру, субструктурні характеристики та напружений стан нанокристалічних іонно-плазмових конденсатів квазібінароної системи WC-TiC |
uk_UA |
dc.type |
Article |
uk_UA |
dc.status |
published earlier |
uk_UA |
Файли у цій статті
Ця стаття з'являється у наступних колекціях
Показати простий запис статті