Post-irradiation helium blistering in copper, austenitic steels and alloys over the temperature interval 0.65-0.95Tmelt

Репозиторій DSpace/Manakin

Показати простий запис статті

dc.contributor.author Kadyrov, H.G.
dc.contributor.author Tsai, K.V.
dc.date.accessioned 2015-03-12T19:57:05Z
dc.date.available 2015-03-12T19:57:05Z
dc.date.issued 2000
dc.identifier.citation Post-irradiation helium blistering in copper, austenitic steels and alloys over the temperature interval 0.65-0.95Tmelt / H.G. Kadyrov , K.V. Tsai // Вопросы атомной науки и техники. — 2000. — № 4. — С. 142-145. — Бібліогр.: 1 назв. — англ. uk_UA
dc.identifier.issn 1562-6016
dc.identifier.uri http://dspace.nbuv.gov.ua/handle/123456789/78209
dc.description.abstract The specimens of copper, austenitic steel 08Cr16Ni15Mo3Nb and nickel-rich 03Cr20Ni45 alloys were irradiated by a-particles (50 MeV, 0.3...3.6 × 10²¹m⁻²) through the special filter-mask and subjected to following thermal treatment at temperatures up to 0.95 × Tmelt for 1...100 h . The helium behavior in the materials was investigated by the methods of scanning electron microscopy and profilimetry of a surface. It was shown that the development of helium bubbles in a closed bulk of the specimens during high-temperature annealing leads to appearing steps on irradiated surfaces followed by flacks and blisters. Migration of helium bubbles in the field of stress gradients causes the nucleation and growth of the long-distance gas-filled cracks. Accumulation of helium bubbles in the cracks leads to lifting of surface layers and formation of a dome-shaped step on the irradiated surface, i.e. the bulk blistering occurs. uk_UA
dc.language.iso en uk_UA
dc.publisher Національний науковий центр «Харківський фізико-технічний інститут» НАН України uk_UA
dc.relation.ispartof Вопросы атомной науки и техники
dc.subject Состояние и проблемы конструкционных материалнов активной зоны реакторов на быстрых нейтронах и термоядерных реакторов uk_UA
dc.title Post-irradiation helium blistering in copper, austenitic steels and alloys over the temperature interval 0.65-0.95Tmelt uk_UA
dc.type Article uk_UA
dc.status published earlier uk_UA
dc.identifier.udc 539.2:539.12.04


Файли у цій статті

Ця стаття з'являється у наступних колекціях

Показати простий запис статті

Пошук


Розширений пошук

Перегляд

Мій обліковий запис