Formation characteristics of Fe₃O₄ magnetic particles precipitated from aqueous solutions and their sorption properties

Репозиторій DSpace/Manakin

Показати простий запис статті

dc.contributor.author Odnovolova, A.M.
dc.contributor.author Sofronov, D.S.
dc.contributor.author Puzan, A.N.
dc.contributor.author Baumer, V.N.
dc.contributor.author Mateychenko, P.V.
dc.contributor.author Desenko, S.M.
dc.contributor.author Vovk, O.M.
dc.contributor.author Mozul', K.A.
dc.contributor.author Bryleva, E.Yu.
dc.date.accessioned 2017-06-07T18:38:16Z
dc.date.available 2017-06-07T18:38:16Z
dc.date.issued 2015
dc.identifier.citation Formation characteristics of Fe₃O₄ magnetic particles precipitated from aqueous solutions and their sorption properties / A.M. Odnovolova, D.S. Sofronov, A.N. Puzan, V.N. Baumer, P.V. Mateychenko, S.M. Desenko, O.M. Vovk, K.A. Mozul', E.Yu. Bryleva // Functional Materials. — 2015. — Т. 22, № 4. — С. 475-481. — Бібліогр.: 13 назв. — англ. uk_UA
dc.identifier.issn 1027-5495
dc.identifier.other DOI: dx.doi.org/10.15407/fm22.04.475 untranslated
dc.identifier.uri http://dspace.nbuv.gov.ua/handle/123456789/119634
dc.description.abstract Effect of temperature and iron concentration in solution on the phase composition, particle size, and magnetization was studied. It is shown that amount of the magnetite phase increases with the temperature increase. The magnetization slightly decreases with increase in the initial iron concentration. It is found that, regardless of the deposition conditions, spherical particles are formed, the average size of which varies within 7 to 15 nm. Comparison between the for removal efficiency and sorption capacity of the particles with the magnetite and hematite phase for cobalt was carried out. The sorption capacity of the particles is essentially independent of the phase composition and is about 18 mg/g for cobalt. For preparation of sorption material based on Fe₃O₄ magnetic particles, it is recommended to carry out the precipitation at the temperature of not lower than 80°C and the concentration of iron in solution of 0.15 to 0.3 M. The resulting particles comprise not less than 90 wt. % of magnetite phase and are characterized by magnetization of 65 to 70 A·m²/kg. uk_UA
dc.language.iso en uk_UA
dc.publisher НТК «Інститут монокристалів» НАН України uk_UA
dc.relation.ispartof Functional Materials
dc.subject Characterization and properties uk_UA
dc.title Formation characteristics of Fe₃O₄ magnetic particles precipitated from aqueous solutions and their sorption properties uk_UA
dc.type Article uk_UA
dc.status published earlier uk_UA


Файли у цій статті

Ця стаття з'являється у наступних колекціях

Показати простий запис статті

Пошук


Розширений пошук

Перегляд

Мій обліковий запис